A zinc oxide/polyurethane-based generator composite as a self-powered sensor for traffic flow monitoring

Submitted by Hamid Souri on

A zinc oxide (ZnO)/polyurethane (PU)-based generator composite was fabricated and its piezoelectric performances were examined in the present work. In addition, the influence of multi-wall carbon nanotubes (MWNTs) and copper powder incorporation on the piezoelectric performance of composites was also studied. The performance level of the composites with various ratios of the constituents was compared in terms of piezoelectric responses obtained from three different tests, i.e., foot stamping, vehicle loading, and cyclic wheel loading tests.