A well‐conditioned and optimally convergent XFEM for 3D linear elastic fracture Submitted by Stephane Bordas on Sat, 11/14/2015 - 16:08 fracture xfem 3D global enrichment conditioning crack growth 3d crack growth A well‐conditioned and optimally convergent XFEM for 3D linear elastic fracture K Agathos, E Chatzi, S Bordas… - International Journal for …, 2015 - Wiley Online Library Read more about A well‐conditioned and optimally convergent XFEM for 3D linear elastic fractureLog in to post comments4219 views