Can you "chop" a mechanical wave?

In this paper we highlight several interesting phenomena that may emerge from coupling simple elastic systems like 1d bars. While in compostes we usually focus on wave propagation normal to the stratification direction (composite layers are coupled in series), here we show that extreme attenuation at multiple frequencies may emerge in linear systems that are coupled transversaly. We also introduce a simple device that act as a chopper for mechanical signals.

http://www.nature.com/articles/s41598-017-16364-8