interface toughness

Role of Interface on the Toughening of Thermoplastic-Based Nanocomposites Reinforced with Nanofibrillated Rubber

Submitted by Mahdi Zeidi on

Optimizing toughening efficiency of nanofibrillated rubber embedded in thermoplastic polymers has always been a challenge. In our work published in Nanoscale journal, by a combined MD-QM method, we demonstrate the roles of interface & interfiber interactions on the toughness and failure mechanisms of rubber-toughened polypropylene nanocomposites.

 

https://doi.org/10.1039/D1NR07363J

 

 

 

Mode II fracture of an elastic-plastic sandwich layer

Submitted by Emilio Martรญneโ€ฆ on

Dear iMechanicians,

Please find below a paper, co-authored with Ivan Cuesta and Norman Fleck, on the mode II fracture of elastic-plastic sandwich layers. The paper is part of the special issue in the Journal of Applied Mechanics dedicated to John Hutchinson's 80th anniversary and the Century Fracture Mechanics Summit.