Compressive performance and crack propagation in Al alloy/Ti2AlC composites

Submitted by Dr. Hanaor - Dโ€ฆ on

The morphology of MAX phase composites is examined here. Specifically, crack branching is examined in Al - Ti2AlC composites showing the role of MAX phase distribution on the fracture performance of such materials. Ductile alloy phases serve to deflect cracks in the hard, yet tough, MAX phase.

Full text available here