Magneto-thermomechanically reprogrammable mechanical metamaterials

Submitted by Joshua on

We developed a method enabling a single material system to transform with untethered, reversible, low-powered reprogrammable deformations and shape locking via the application of magneto-thermomechanically triggered prestress on the Shape Memory Polymers (SMPs) and structural instability with asymmetric magnetic torque. The mutual assistance of two physics conceptsโ€”magnetic control combined with the thermomechanical behavior of SMPs is demonstrated, without requiring new materials synthesis and high-power energy for reprogramming.