Morphing Matter

Fan Xu's picture

Computational morphology and morphogenesis for empowering soft-matter engineering

Morphing soft matter, which is capable of changing its shape and function in response to stimuli, has wide-ranging applications in robotics, medicine and biology. Recently, computational models have accelerated its development. Here, we highlight advances and challenges in developing computational techniques, and explore the potential applications enabled by such models.

Yifan Yang, Fan Xu*

Nature Computational Science, 2024, https://doi.org/10.1038/s43588-024-00647-y

Fan Xu's picture

SES 2024 Call for abstract: MS 10.11 Morphing Matters: Inspiration, Mechanics, Computation, Design, Fabrication, and Applications

Dear Colleagues,

We would like to invite you to submit abstracts and attend the minisymposium titled "10.11 Morphing Matters: Inspiration, Mechanics, Computation, Design, Fabrication, and Applications" in the 2024 SES Annual Techinical Meeting, August 20-23, 2024, Hangzhou, China.

https://www.2024ses.com/

Abstract submissions are due April 1, 2024.

 

10.11 Morphing Matters: Inspiration, Mechanics, Computation, Design, Fabrication, and Applications

Teng zhang's picture

SES 2023 Symposium 9-3 - Morphing Matter: Bioinspiration, Computational Design, Fabrication, Mechanics, and Sustainability

Morphing matter includes biological and engineering materials and structures with dynamic and tunable properties such as shape, color, stiffness, texture, and density. Examples include pinecones that open when dried and close when wet, octopus that camouflages by changing body shapes, textures and colors, food that changes shapes during cooking, and smart windows that dynamically tune color and surface roughness.