Extreme Particle Shape Effect for Packs of Platonic Solids

For centuries, great minds like Kepler, Maxwell and Einstein have investigated the statistical characterization of many-body systems, and implications of small-scale structures on the macroscopic transport and mechanical properties. In this work, an accurate statistical description of heterogeneous particulate materials is computed using novel adaptive interpolation/integration scheme. This statistical information is then utilized within mathematical theories for predicting the overall thermo-mechanical behavior.