Skip to main content

Teng Li Group Research

Determining Graphene Adhesion via Substrate-regulated Morphology of Graphene

Submitted by Teng Li on

Understanding the adhesion between graphene and other materials is crucial for achieving more reliable graphene-based applications in electronic devices and nanocomposites. The ultra-thin profile of graphene, however, poses significant challenge to direct measurement of its adhesion property using conventional approaches. We show that there is a strong correlation between the morphology of graphene on a compliant substrate with patterned surface and the graphene-substrate adhesion.