Effect of constraint on swelling of hydrogels and formation of surface creases

Submitted by Rui Huang on

Inspired by recent works by Wei Hong , Xuanhe Zhao, Zhigang Suo, and their coworkers, we started a project on hydrogels, with particular interest in various instability patterns observed in experiments. The attachment is our first manuscript on this subject. Through this work we hope to achieve the following:

Failure Criteria for Fiber Analysis

Submitted by ash74u on

Hello,

I am trying to include a failure criteria for a single yarn in a plain- weave fabric model.The yarns behave as elastic-brittle( That is there is no plastic deformation)

I have the failure stresses and strains data in both fiber and transverse directions.I have  included the following properties:

Material definition

Density

Elastic : engineering constants

Viscoelastic: Relaxation test data

Analysis of Torsion-Bending of Laminated Composite Beam by FEM using ANSYS

Submitted by Ryan Mendez Cabrera on

 Hi everyone!

i'm a researcher at the Deparment of Mechanical Engineering of University of the Philippines-Diliman. currently, i'm working on completing my thesis for my MS degree. my research area in general is in mechanics of composite materials (fiber-reinforced). my problem is that of formulating the FEM solution to the torsion-bending of laminated composite beam having orthotropic layers.

Deformation gradients and atomistic simulations

Submitted by Biswajit Banerjee on

I came upon a recent paper called "Deformation gradients for continuum mechanical analysis of atomistic simulations" by Jonathan A. Zimmerman , Douglas J. Bammann,  and Huajian Gao, International Journal of Solids and Structures 46 (2009) 238–253 where the authors conclude with

User Element for Ansys

Submitted by jimmy on

Hi,

I ask for help. I need to implement a user element for shell element in Ansys, and I ask if somebody know how to do this or can send me some example. I try to read something but I not found a good example about user element in Ansys Thanks a lot.

Simple beam simulation in Abaqus

Submitted by Emmanuel E. Ufuah on

Hi everyone,

I have modelled a simple beam using continuum elements to assess the mechanical behaviour. The results are quite good since it could predict deflection close to test data. Using ABAQUS general-purpose shell elements, the deflection is quite small compared to test results ie it appears the material has become more stiff. Can any one give me a clue?

Many thanks in advance,

Emmanuel  

 

Combined EAM and Stillinger-Weber potential and Combined EAM and Tersoff Potential

Submitted by Anonymous (not verified) on