Anisotropy and variability in polyurethane foams: experiments and modeling Submitted by Biswajit Banerjee on Wed, 01/23/2013 - 23:05 research Plasticity foam anisotropy Constitutive model expermental data Authors: B. Kraus, R. Das, B. Banerjee Abstract: Read more about Anisotropy and variability in polyurethane foams: experiments and modelingLog in to post comments5667 views