characteristic Length

Submitted by m0435117 on

Hi

 

is there a way to get the characteristic length of one element? I wanna calculate xult (when the element is cracked, fracutred..). 

 I use the concrete damage plasticity model and after reaching the tensile strength i assume a linear softening with fracture energy.

 

Input are:

   Youngยดs modulus

   max. tensile strength

   fracture energy

 

Outpu:

   when do i reach xult or what is the plastic strain equivalent