Hi All,

I want to use ductile damage model in ABAQUS to model the damage of thermoplastic polymers, in which I need to input the damage evolution law (\dot{d}).

My question is on the way we have to measure the variable d.

Suppose I have 10 cycles of load-unload test. For slope of the first load will be initial Young's modulus at undamaged state E_0. now for the next cycle, which part of the curve we need to measure their slope to get the damage variable (d = 1 - E/E_0).

Summer School on Fatigue and Damage Mechanics of Composite Materials

Submitted by michele.zappal… on

Dear Colleagues,

we are glad to present the Summer School on Fatigue and Damage Mechanics of Composite Materials (13 . 17 July 2015) and the Short Course on Experimental Techniques and Testing of Composite Materials (9 . 10 July 2015) organized by and to be held at The Department of Management and Engineering  - University of Padova in Vicenza - Italy.

Summer School on Fatigue and Damage Mechanics of Composite Materials

Submitted by michele.zappal… on

Dear Colleagues,

we are glad to present the Summer School on Fatigue and Damage Mechanics of Composite Materials (13 . 17 July 2015) and the Short Course on Experimental Techniques and Testing of Composite Materials (9 . 10 July 2015) organized by and to be held at The Department of Management and Engineering  - University of Padova in Vicenza - Italy.

Post-doc position on computational mechanics at IMT Lucca

Submitted by marco.paggi on

A new post-doc position (1 year renewable up to 3 years, till the end of the ERC Starting Grant Project CA2PVM, http://musam.imtlucca.it/CA2PVM.html ) is open in the Research Unit MUSAM - Multi-scale Analysis of Materials ( http://musam.imtlucca.it ) directed by Prof.

Postdoctoral Position in Computational Damage Mechanics Available at Masdar Institute in Abu Dhabi

Submitted by Rashid K. Abu Al-Rub on

A Postdoctoral Research Fellow position in computational damage mechanics is
available immediately at Masdar Institute of Science and Technology in Abu
Dhabi in United Arab Emirates. Masdar Institute is established in collaboration
with Massachusetts Institute of Technology. The research project focuses on
using advanced computational fracture and damage mechanics for simulating the
behavior of advanced materials under different loading and environmental
conditions. The candidate is expected to have a PhD in the field of Mechanical,
Civil, or Aerospace Engineering with solid knowledge of theoretical/computational
solid mechanics; continuum damage mechanics, fracture mechanics,

Call of interest - Post-doc position at IMT Lucca on computational mechanics for photovoltaic applications

Submitted by marco.paggi on
This is a call of interest for a post-doc position (1 year renewable up to 3 years) at the IMT Institute for Advanced Studies Lucca, Italy (www.imtlucca.it), in the field of computational damage and fracture mechanics. The activities are in the framework of the ERC Starting Grant IDEAS "Multi-field and multi-scale Computational Approach to design and durability of Photovoltaic Modules" (Prof. Paggi, Principal Investigator).

For more details about the project, see:

Postdoctoral Position in Hydraulic Fracture Mechanics Available at Masdar Institute in Abu Dhabi

Submitted by Rashid K. Abu Al-Rub on

Postdoctoral Research Fellow position in hydro-fracturing (fracking) is
available immediately at Masdar Institute of Science and Technology in Abu
Dhabi in United Arab Emirates. Masdar Institute is established in collaboration
with Massachusetts Institute of Technology. The research project focuses on
using advanced computational fracture and damage mechanics for simulating
hydro-fracturing of rocks in hydrocarbon fields. The candidate is expected to
have a PhD in the field of geomechanics, or civil engineering with solid
knowledge of hydraulic fracture mechanics and excellent theoretical and

Grants for Workshop on "Physics-based fracture and damage mechanics" in Antalya/Turkey, May 15-17, 2013

Submitted by Kalle Nilsson on

We would like to inform you about a Workshop on "Physics-based fracture and damage mechanics" in Antalya/Turkey, May 15-17, 2013.

The workshop is co-organized by the Joint Research Centre (European Commission) and TOBB University of Economics and Technology. The Workshop is funded by the European Commission’s Integration and Enlargement Action. The participants from target countries* (citizen of or working in a target country) can be fully financially supported by the European Commission.

Full scholarships available at European Commission funded workshop on fracture and damage mechanics in Antalya / Turkey

Submitted by Tuncay Yalcinkaya on

European Commission' s JRC (Joint Research Centre) is organizing the 2nd workshop on physics based modeling of material properties and experimental observations in collaboration with TOBB University of Economics and Technology. The workshop will be held in Antalya/Turkey on 15-17 May 2013, and the special focus will be fracture and damage mechanics.