Molecular Dynamics Analysis of the Thermal Conductivity of Graphene and Silicene Monolayers of Different Lengths Submitted by Jingjie Yeo on Fri, 05/09/2014 - 07:50 research molecular dynamics graphene phonon LAMMPS graphene sheet Thermal conductivity phonon density of states silicene silicene sheet phonon dispersion Tersoff potential http://dx.doi.org/10.1166/jctn.2014.3568 Read more about Molecular Dynamics Analysis of the Thermal Conductivity of Graphene and Silicene Monolayers of Different LengthsLog in to post comments5143 views