Skip to main content

Mechanical characterization and micromechanical modeling of bread dough. J.Rheol [http://dx.doi.org/10.1122/1.4768463]

Submitted by fendi on

The mechanical behavior of dough, gluten, and
starch was studied in an effort to investigate whether bread dough can be
treated as a two phase (starch and gluten) composite material. Mechanical
loading tests revealed rate-dependent behavior for both the starch and the
gluten constituents of dough. There is evidence from cryo-scanning electron
microscopy that damage in the form of debonding between starch and gluten
occurs when the sample is stretched. In addition, the Lodge material model was
found to deviate from the tension and shear stress-strain test data by a

Multiple Ph.D. Positions in Mechanics of Soft Materials at Michigan State University

Submitted by Roozbehdar on

The recently founded Group of Appleid mechanics in Enviormental & Civil Engineering Department at Michigan State University has a few openings for PhD positions to work on Multiscale Modeling of Soft Materials starting Fall 2014.

Virtual Special Issue: CFD simulation of pedestrian-level wind conditions around buildings: past achievements and prospects

Submitted by Laure Ballu on

This Virtual Specail Issue deals with papers on CFD simulation of pedestrian-level wind conditions around buildings, published in the Journal of Wind Engineering and Industrial Aerodynamics (JWEIA).

Force and stroke of a hydrogel actuator

Submitted by Widusha Illeperuma on

Hydrogels that undergo a volume phase transition in response to an
external stimulus are of great interest because of their possible use as
actuator materials. The performance of an actuator material is normally
characterized by its force–stroke curve, but little is known about the
force–stroke behavior of hydrogels. We use the theory of the ideal
elastomeric gel to predict the force–stroke curves of a
temperature-sensitive hydrogel and introduce an experimental method for
measuring the curve. The technique is applied to PNIPAm hydrogels with
low cross-link densities. The maximum force generated by the hydrogel
increases with increasing cross-link density, while the maximum stroke

Faculty position in computational materials science and engineering at Illinois Institute of Technology

Submitted by MMAEatIIT on

Applications are invited for a tenure-track faculty position at the assistant or associate professor level in the area of computational materials science and engineering. Candidates from a range of disciplines such as materials science, chemistry, physics, chemical engineering, and mechanical engineering are all welcome to apply.

Faculty Position in Biomechanics / Bioengineering in Dept. of Mechanical Engineering at University of Colorado, Boulder

Submitted by VirginiaLFerguson on

The Department of Mechanical Engineering at the University of Colorado Boulder invites applications for a tenure-track faculty position in the area of Bioengineering with an emphasis on mechanics and/or design.

Biomechanics areas of interest include, but are not limited to, theoretical, experimental, and computational biomechanics and/or mechanobiology. Design areas include, but are not limited to, photoacoustics and ultrasonics, theranostics, biorobotics and/or medical device design.

Workshop "Impact of mechanical and thermal loads on the long term stability of PV modules" on 05th Nov.2013, Hamelin, Germany

Submitted by J.Reinoso on

Dear imechanica members, 

 

I am glat to inform your the organization of the workshop  "Impact of mechanical and thermal loads on the long term stability of PV modules" on 05th November 2013 at ISFH (Institute for Solar Energy Research Hamelin), in Hamelin, Germany.