I invite you to submit an abstract in the broad field of Composites Manufacturing and 3D Printing to the MS 218, EMI 2020 to be held at Columbia University in New York. The deadline for submitting abstracts is Jan 15. 2020. The outline for this mini-symposia is attached.

 

Best Regards,

Elyas Goli

UIUC

 

 

Scholarships for Postgraduate Research Students to study at Swinburne University of Technology in Australia

Submitted by tsekm on

There are several PhD scholarships at School of Engineering, Swinburne University of Technology, Australia. The scholarship includes the annual stipend AU$27,596 for three years (with possible 6 months extension). The focus of the research will be on topology optimization of structures, materials, and metamaterials.

To be successful in this role you will need to demonstrate the following:

1)    A Bachelor degree honours and/or a research master’s degree in mechanical engineering, civil engineering, applied mathematics, or a related field;

RA positions available at Penn State

Submitted by Sulin Zhang on

My research group has two RA positions openings in the near term.

One position is in the area of experimental mechanobiology, where we develop force sensors, measure mechanical force history of cells and tissues in vitro, and correlate the force history to cell functions. We target this RA position to be filled in Spring 2020. 

Postdoc Positions at Jiangsu University, Zhenjiang, China

Submitted by zhujg on

Postdoc positions are available in the group of Prof. JG Zhu at Jiangsu University, Zhenjiang, China. Those possessing PhDs in the area of solid experimental mechanics are sought. We are particularly interested in candidates with experience in experimental measurements and nondestructive techniques.

PhD Positions in Mechanical Engineering at NJIT for Fall 2020

Submitted by sfarokhirad on

There are PhD positions at RAD Lab in the Department of Mechanical and Industrial Engineering at New
Jersey Institute of Technology (NJIT). The focus of the research will be on creating novel computational
and theoretical models for the dynamics of complex fluids with particular emphasis on particle-laden multiphase flows and biological flows of active matter in the living systems.

Friction-induced energy losses in mechanical contacts subject to random vibrations

Submitted by Antonio Papangelo on

In this paper, we apply the previously developed Method of Memory Diagrams (MMD) to the description of an axisymmetric mechanical contact with friction subject to random vibrations. The MMD belongs to a family of semi-analytical methods of contact mechanics originating from the classical Cattaneo-Mindlin solution; it allows one to efficiently compute mechanical and energetic responses to complex excitation signals such as random or acoustic ones.

A coarse-graining approach for modeling nonlinear mechanical behavior of FCC nano-crystals

Submitted by M. Jahanshahi on

The ever-increasing growth of nano-technology has elevated the necessity for development of new computational methods that are capable of evaluating large systems at nano-scale. The existing techniques, such as the molecular dynamics, lack the ability to simulate large systems of practical size and time scales. In order to provide a realistic simulation of large models, the multi-scale methods such as coarse-graining, have therefore become very popular. The coarse-grained models have mostly been used to simulate large biomolecules, such as proteins, lipids, DNA and polymers.

Universal Displacements in Linear Elasticity

Submitted by arash_yavari on

In nonlinear elasticity, universal deformations are the deformations that exist for arbitrary strain-energy density functions and suitable tractions at the boundaries. Here, we discuss the equivalent problem for linear elasticity. We characterize the universal displacements of  linear elasticity: those displacement fields that can be maintained by applying boundary tractions in the absence of body forces for any linear elastic solid in a given anisotropy class.

Materials Division events at IMECE and newsletter

Submitted by Yong Zhu on

Dear Colleagues,

During the ASME-IMECE next week, the Materials Division will host a number of events including plenary lectures, award lectures, and reception. You are cordially invited to these events. 

Track 10 Plenary Sessions:

Zhigang Suo – Tuesday, Nov. 12th, 9:45–10:30 am, Room 255F, Convention Center  

Irene Beyerlein – Wednesday, Nov. 13th, 9:45–10:30 am, Room 155F, Convention Center

 

Award Lectures/Reception (Tuesday, November 12):