Graphene is the world's thinnest material.

The one-atom-thick carbon layers have shown remarkable strength and stiffness.

The so-called "graphene-based sheets" can be mixed into polymers, glasses and ceramics, to produce novel composite materials with useful thermal, electrical and mechanical properties.

The team led by Professor Andre Geim at The University of Manchester, extracted individual planes of carbon atoms from graphite crystals, which resulted in the production of the thinnest possible fabric - graphene.

The resulting atomic sheet is stable, highly flexible and strong and remarkably conductive. 