A molecular dynamics based investigation of thermally vibrating graphene under different boundary conditions Submitted by rrahman on Mon, 04/20/2015 - 14:54 research molecular dynamics graphene Thermal vibration LAMMPS continuum plate theory ripples FFT R. Rahman and J.T. Foster Read more about A molecular dynamics based investigation of thermally vibrating graphene under different boundary conditionsLog in to post comments3684 views