The effect of porosity on the stiffness and fracture energy of brittle organosilicates

Submitted by Li Han on

Integrating porous low-permittivity dielectrics into Cu metallization is one of the strategies to reduce power consumption, signal propagation delays, and crosstalk between interconnects for the next generation of integrated circuits. However, the porosity and pore structure of these low-k dielectric materials also strongly affects other important material properties besides their dielectric constant.