Skip to main content

ABAQUS

Composite Solid

Submitted by JM-UofR on

Hi All,

I am analysing a fiber composite solid plate with a large and small holes. The model is meshed with C3D8R elements. The output has U and RF in global CSYS and S, E in local CSYS. I have problem in reading  S and E written in local CSYS. I know it is very simple, but I cant able to figure it out. Those who know, how to read the S and E in local CSYS, please help me. Tks in advance for your time and advice.

Regrads

Jacob 

difficulties CONTACT problem with plasticity using ABAQUS FEA code.

Submitted by lazghabt on

Hello everyone:

1.  I have built a FEM model 2D plane strain using ABAQUS/Standard (CPE4R) elements,

2. I am  modeling the contact between a cylinder and a plate in 2D.

3. The Cylinder material is given is ELASTIC ISOTROPIC material with no plasticit E=310 GPa

4.  The plate is with a Ramberg-Osgood plasticity with a Young's modulus E=210 GPa.

5. The mesh at the the contact point is VERY refined element characteristic length is about 1 micron. (My model units are  (mm,N,sec)).

Abaqus / polymer simulation

Submitted by poucinette on
Hi all,



I'm trying to model a peel T test on a composite material composed of steel and polymer (polypropylen) on Abaqus 6.7. Between these parts, there are cohesive elements COH3D8.

I have a problem with my model and I don't understand it. You can visualize my results in attachs files.

For understand this draw, a few precisions:

The elements in white has just here to guide the materials.

In B (cf attachs files), the nodes are embedded.

In A I applied a velocity.

Extended Chaboche viscoplastic model for cyclic loading

Submitted by Fatigueless on
Choose a channel featured in the header of iMechanica

These days I've been applying oneself to implement the Chaboche viscoplastic model in ABAQUS user-subroutine for simulating the cyclic loading in single crystals.

The procedure can easily get out. I'm not sure about the problem, the deduction of Jacobian, the convergence? 

Btw, I know there is free subroutine for crystal plasticity by Huang YG. I wonder if the UMAT routine for chaboche model is available, then I can generalize it to fit for my case.

EFD or CFD Softwares Help

Submitted by projpeixe on

Please, I need some EFD or CFD software that has an Student Version. I have to make an analysis Solid-Fluid and vice versa, but i have no software to make that.

Now I'm using Pro/E to make Streches and statics analysis, but i cant do any EFD or CFD without any patch or software.  Anyone knows any?

 

Tanks! 

Sharing ABAQUS UMAT and VUMAT subroutines

Submitted by azadpoor on
Choose a channel featured in the header of iMechanica

I have noticed that a lot of people are using UMAT and VUMAT material model
subroutines for their researches. However, most of these subroutines do not
find their way to free code market and remain in the hands of the developers.
Therefore, a lot of wheel re-inventing has to be done by other people. Since
development and testing of a material subroutine takes a damn long time, I
think it is a good idea if each of us can share the subroutines she has
developed with the others. I know that a couple of subroutines are publicly

Sharing ABAQUS UMAT and VUMAT subroutines

Submitted by azadpoor on

I have noticed that a lot of people are using UMAT and VUMAT material model
subroutines for their researches. However, most of these subroutines do not
find their way to free code market and remain in the hands of the developers.
Therefore, a lot of wheel re-inventing has to be done by other people. Since
development and testing of a material subroutine takes a damn long time, I
think it is a good idea if each of us can share the subroutines she has
developed with the others. I know that a couple of subroutines are publicly