Recent paper is Part-2 of the paper mentioned below
http://imechanica.org/node/10104
http://www.sciencedirect.com/science/article/pii/S0749641910001142
Mechanical responses and deformation mechanisms of an AZ31 Mg alloy sheet under dynamic and simple shear deformations
Abstract
Recent comments