Yield surface,Texture, and Deformation mechanisms in AA5754 Submitted by Amit Pandey on Fri, 03/15/2013 - 19:53 research Plasticity Textures dynamic strain rate Experimental and numerical investigations of yield surface, texture, and deformation mechanisms in AA5754 over low to high temperatures and strain rates Read more about Yield surface,Texture, and Deformation mechanisms in AA5754Log in to post comments4670 views
Mechanical response and texture evolution in magnesium alloy Submitted by Amit Pandey on Fri, 04/15/2011 - 01:59 research magnesium alloys Textures Abstract Read more about Mechanical response and texture evolution in magnesium alloy 2 commentsLog in to post comments7206 views