Influence of anisotropic elasticity on the mechanical properties of fivefold twinned nanowires
In this paper in the Journal of the Mechanics and Physics of Solids (vol. 84, p. 358,
http://authors.elsevier.com/a/1Rk5057Zjdx-o ) we propose a
new theory for the mechanical properties of fivefold twinned nanowires.
We show that the Frank vector of the central wedge disclination depends on the uniaxial strain,