In Situ Atomic-Scale Observation of Twinning Dominated Deformation in Nanoscale Body-Centred Cubic Tungsten

Submitted by Jiangwei Wang on

In situ atomic-scale observation of twinning-dominated deformation in nanoscale body-centred cubic โ€‹tungsten

By Jiangwei Wang, Zhi Zeng, Christopher R. Weinberger, Ze Zhang, Ting Zhu & Scott X. Mao

Nature Materials (2015) doi:10.1038/nmat4228

http://www.nature.com/nmat/journal/vaop/ncurrent/full/nmat4228.html