Skip to main content

mixture

Tunable electrical and mechanical responses of PDMS and polypyrrole nanowire composites

Submitted by duping812 on

doi:10.1088/0022-3727/46/19/195303

A generic experimental procedure is presented in this work to enhance
the electrical responses of polydimethylsiloxane (PDMS) through
incorporation of conducting polymer nanowires, while maintaining the
desirable mechanical flexibility of PDMS. The conducting polypyrrole