Skip to main content

Statistics of Electromigration Lifetime Analyzed Using a Deterministic Transient Model

Submitted by Jun He on

The electromigration lifetime is measured for a large number of copper lines encapsulated in an organosilicate glass low-permittivity dielectric. Three testing variables are used: the line length, the electric current density, and the temperature. A copper line fails if a void near the upstream via grows to a critical volume that blocks the electric current. The critical volume varies from line to line, depending on line-end designs and chance variations in the microstructure. However, the statistical distribution of the critical volume (DCV) is expected to be independent of the testing variables. By contrast, the distribution of the lifetime (DLT) strongly depends on the testing variables. For a void to grow a substantial volume, the diffusion process averages over many grains along the line. Consequently, the void volume as a function of time, V(t), is insensitive to chance variations in the microstructure. As a simplification, we assume that the function V(t) is deterministic, and calculate this function using a transient model. We use the function V(t) to convert the experimentally measured DLT to the DCV. The same DCV predicts the DLT under untested conditions.

Variability in Bone Indentation

Submitted by MichelleLOyen on

A viscous-elastic-plastic indentation model was used to assess the local variability of properties in healing porcine bone. Constant loading- and unloading-rate depth-sensing indentation tests were performed and properties were computed from nonlinear curve-fits of the unloading displacement-time data. Three properties were obtained from the fit: modulus (the coefficient of an elastic reversible process), hardness (the coefficient of a nonreversible, time-independent process) and viscosity (the coefficient of a nonreversible, time-dependent process). The region adjacent to the dental implant interface demonstrated a slightly depressed elastic modulus along with an increase in local time-dependence (lower viscosity); there was no clear trend in bone hardness with respect to the implant interface.

Environmental Effects on Crack Characteristics for OSG Interconnect Materials

Submitted by Jeannette Jacques on

Jeannette M. Jacques, Ting Y. Tsui, Andrew J. McKerrow, and Robert Kraft

To improve capacitance delay performance of the advanced back-end-of-line (BEOL) structures, low dielectric constant organosilicate glass (OSG) has emerged as the predominant choice for intermetal insulator. The material has a characteristic tensile residual stress and low fracture toughness. A potential failure mechanism for this class of low-k dielectric films is catastrophic fracture due to channel cracking. During fabrication, channel cracks can also form in a time-dependent manner due to exposure to a particular environmental condition, commonly known as stress-corrosion cracking. Within this work, the environmental impacts of pressure, ambient, temperature, solution pH, and solvents upon the channel cracking of OSG thin films are characterized. Storage under high vacuum conditions and exposure to flowing dry nitrogen gas can significantly lower crack propagation rates. Cracking rates experience little fluctuation as a function of solution pH; however, exposure to aqueous solutions can increase the growth rate by three orders of magnitude.

Dynamics of terraces on a silicon surface due to the combined action of strain and electric current

Submitted by Wei Hong on

A (001) surface of silicon consists of terraces of two variants, which have an identical atomic structure, except for a 90° rotation. We formulate a model to evolve the terraces under the combined action of electric current and applied strain. The electric current motivates adatoms to diffuse by a wind force, while the applied strain motivates adatoms to diffuse by changing the concentration of adatoms in equilibrium with each step. To promote one variant of terraces over the other, the wind force acts on the anisotropy in diffusivity, and the applied strain acts on the anisotropy in surface stress. Our model reproduces experimental observations of stationary states, in which the relative width of the two variants becomes independent of time. Our model also predicts a new instability, in which a small change in experimental variables (e.g., the applied strain and the electric current) may cause a large change in the relative width of the two variants.

Laser Annealing of Amorphous NiTi Shape Memory Alloy Thin Films to Locally Induce Shape Memory Properties

Submitted by Xi Wang on

Xi Wang, Yves Bellouard, Joost J. Vlassak

Published in Acta Materialia 53 (2005) p4955-4961.

Abstract — We present the results of a crystallization study on NiTi shape memory thin films in which amorphous films are annealed by a scanning laser. This technique has the advantage that shape memory properties can be spatially distributed as required by the application. A kinetics study shows that nucleation of the crystalline phase occurs homogenously in the films. Consequently, the laser annealing process produces polycrystalline films with a random crystallographic texture. The crystallized films have a uniform microstructure across the annealed areas. The material in the crystalline regions transforms reversibly to martensite on cooling from elevated temperature and stress measurements show that a significant recovery stress is achieved in the films upon transformation.

Nanoscale Intracellular Organization and Functional Architecture Mediating Cellular Behavior

Submitted by prleduc on

Cells function based on a complex set of interactions that control pathways resulting in ultimate cell fates including proliferation, differentiation, and apoptosis. The interworkings of his immensely dense network of intracellular molecules are influenced by more than random protein and nucleic acid distribution where their interactions culminate in distinct cellular function.

Pattern Effect on Low-k Channel Cracking

Submitted by Xiao Hu Liu on

Low dielectric constant (low-k) is achieved often at the cost of degraded mechanical properties, making it difficult to integrate the dielectric in the back end of line (BEOL) and to package low-k chips. Development of low-k technology becomes costly and time-consuming. Therefore, more frequently than before, people resort to modeling to understand mechanical issues and avoid failures. In this paper we present three multilevel patterned film models to examine channel cracking in low-k BEOL. The effects of copper features, caps and multilevel interconnects are investigated and their implications to BEOL fabrication are discussed.

Low-k BEOL Mechanical Modeling
Liu, Xiao Hu; Lane, Michael W; Shaw, Thomas M; Liniger, Eric G; Rosenberg, Robert R; Edelstein, Daniel C
Advanced Metallization Conference 2004 (AMC 2004); San Diego, CA and Tokyo; USa and Japan; 19-21 Oct. 2004 and 28-29 Sept. 2004. pp. 361-367. 2005

Faculty Position at Duke University

Submitted by John E. Dolbow on

DEPARTMENT OF MECHANICAL ENGINEERING AND MATERIALS SCIENCE

PRATT SCHOOL OF ENGINEERING

The Department of Mechanical Engineering and Materials Science invites applications for tenure-track faculty positions. Two tenure-track appointments are anticipated and are open to all ranks, Assistant, Associate and Full Professor level. Applications are invited from candidates with research interests in autonomous vehicles and robotic systems, conventional and alternative energy technology, and MEMS/NEMS devices. Applications will also be accepted for allied mechanical engineering disciplines such as nonlinear dynamics and control, sensor technology, small and micro-scale propulsion systems, aerodynamics and aeroelasticity, thermal sciences, and vehicle dynamics.

Successful candidates are expected to establish a vibrant research program, obtain competitive external research funding, and participate actively in teaching at both the undergraduate and graduate levels. Applicants should submit a cover letter describing their research interests and qualifications, a curriculum vitae, and the names and addresses of three references. Please submit your application to mems-search [at] mems.duke.edu as a PDF (preferred) or Word file attached to your email. Duke University is an Affirmative Action/Equal Opportunity Employer.

Nanoscale incipient asperity sliding and interface micro-slip assessed by the measurement of tangential contact stiffness

Submitted by Yanfei Gao on

Experiments with a multidimensional nano-contact system (Lucas, Hay, and Oliver, J. Mater. Res. 2004) have shown that, prior to kinetic frictional sliding, there is a significant reduction of the tangential contact stiffness relative to the elastic prediction. The reduction occurs at contact sizes below about 50~200nm for aluminum single crystals and several other materials. Using a cohesive interface model, we find that this reduction corresponds to a transition from a small-scale-slip to large-scale-slip condition of the interface.