Submitted by Bin Wang on

Layered and scrolled nanocomposites with aligned semi-infinite graphene inclusions at the platelet limit, Liu, et al. Strano, Science, 2016

Novelty/impact/significance:

A stacking and folding method (semi-infinite graphene/polycarbonate (Gr/PC) films, exponential increase in thickness with quadrant fold) to generate aligned Gr/PC composites (~320 layers) that have superior modulus and strength at exceptionally low volume fraction of Gr.

Shuman Xia is the recipient of the 2020 Eshelby Mechanics Award for Young Faculty

Submitted by Executive Comm… on

It is with great pleasure that we announce the outcome of the 2020 competition for the Eshelby Mechanics Award for Young Faculty. The recipient of the 2020 award is Professor Shuman Xia, from Georgia Tech. This award is given annually to rapidly emerging junior faculty who exemplify the creative use and development of mechanics. The intent of the award is to promote the field of mechanics, especially among young researchers.

ASME IMECE 2020 Mechanics of Soft Materials symposium

Submitted by Yuhang Hu on

A few updates about the ASME IMECE 2020 Mechanics of Soft Materials symposium:

 

•            IMECE 2020 will be fully online with the technical meetings held during the week of November 15. IMECE remains the same otherwise. The online format will leverage the extra capabilities that come from a virtual setting.

Immediate Postdoc Position in Soft Robotics at NCSU

Submitted by Jie. Yin on

Applications are invited for an immediate postdoctoral associate opening in the broad area of soft robotics in the Applied Mechanics of Materials Lab of Mechanical and Aerospace Engineering Department at North Carolina State University, Raleigh, NC, US.

This project will focus on bioinspired multifunctional high-performance soft robots in manipulation and locomotion.   

EML Webinar by Prof. Yonggang Huang on relation between blood pressure and pulse wave velocity

Submitted by Teng Li on

EML Webinar on July 22, 2020 will be given by Professor Yonggang Huang, Northwestern University via Zoom meeting. Discussion leader: Vicky Nguyen, Johns Hopkins University.

Title: Relation between blood pressure and pulse wave velocity

Time: 7 am California, 10 am Boston, 3 pm London, 10 pm Beijing on July 22, 2020

PhD student or postdoc position in “Atomistic Computer Simulation of Grain Boundary Structure and Mechanics”

Submitted by TobiasBrink on

The Max-Planck-Institut für Eisenforschung (Düsseldorf, Germany) offers a position in the department Structure and Nano-/Micromechanics of Materials (Prof. G. Dehm): PhD student or postdoc position in “Atomistic Computer Simulation of Grain Boundary Structure and Mechanics”

Understanding how grain boundaries influence plasticity will lead to significant advances in material design. In the context of the department’s research, the overarching aim of this PhD project is to connect grain boundary structures in fcc metals to physical properties.

Soterix Medical: Individualized Modeling & Planning for Stroke Treatment

Submitted by Philippe on

Transcranial direct current stimulation (tDCS) benefits from individualized 3D modelling and simulation. I recommend anyone wanting to learn more about work in these area check out this webinar on July 30th:

https://register.gotowebinar.com/register/556126791558271247?source=IMechanica