Kinematic hardening analysis of Li-ion battery with concentration-dependent material behaviours under cyclic charging
Kinematic hardening analysis of Li-ion battery with concentration-dependent material behaviours under cyclic charging and discharging
A.KaramiA.Nayebi, https://doi.org/10.1016/j.jpowsour.2020.228155Highlights
- •
-
The diffusion equation with the variable coefficient is solved numerically.