Skip to main content

Postdoctoral position in experimental additive manufacturing and characterization of nickel-titanium shape memory alloys

Submitted by wael.zaki on

Location

Khalifa University of Science and Technology, main campus, Abu Dhabi, UAE. Website: www.ku.ac.ae

Duration

The position is available from September 2019 for up to 34 months. 

About the role

Laser manipulated wrinkling patterns

Submitted by Fan Xu on

Smart soft materials, because of their mechanical flexibility and quick response to multi-physics stimuli, have drawn considerable attention over the past few years. Here, we present controllable wrinkling patterns of a liquid crystal polymer film attached on a soft substrate, controlled by laser illumination that holds unique optical characteristics of high coherence and irradiance.

Random fiber networks with inclusions: The mechanism of reinforcement

Submitted by Mohammad Refat… on

The mechanical behavior of athermal random fiber networks embedding particulate inclusions is studied in this work. Composites in which the filler size is comparable with the mean segment length of the network are considered. Inclusions are randomly distributed in the network at various volume fractions, and cases in which fibers are rigidly bonded to fillers and in which no such bonding is imposed are studied separately. In the presence of inclusions, the small strain modulus increases, while the ability of the network to strain stiffen decreases relative to the unfilled network case.

Continuum mechanics of moving defects in growing bodies

Submitted by Amit Acharya on

Amit Acharya          Shankar Venkataramani

 (In Materials Theory)

Growth processes in many living organisms create thin, soft materials with an intrinsically hyperbolic
geometry. These objects support novel types of mesoscopic defects - discontinuity lines
for the second derivative and branch points - terminating defects for these line discontinuities.
These higher-order defects move "easily", and thus confer a great degree of
flexibility to thin hyperbolic elastic sheets. We develop a general, higher-order, continuum mechanical framework
from which we can derive the dynamics of higher order defects in a thermodynamically consistent
manner. We illustrate our framework by obtaining the explicit equations for the dynamics
of branch points in an elastic body.

 

https://www.researchgate.net/publication/333877242_Continuum_mechanics_of_moving_defects_in_growing_bodies

Postdoc in theory and simulation of active matter, cell and tissue mechanobiology in Barcelona

Submitted by Marino Arroyo on

The group on “Mechanics of soft and living interfaces” (https://www.lacan.upc.edu/mechanics-of-soft-and-living-interfaces/) lead by Marino Arroyo (https://www.lacan.upc.edu/arroyo/) is looking for a highly motivated and creative postdoctoral researcher to study the mechanical organization of epithelial cells and tissues, and how this understanding can lead to a precise control of tissue structure, mechanical properties, and dynamics.

Modeling Uncertainties in Molecular Dynamics Simulations Using A Stochastic Reduced-Order Basis

Submitted by Haoran Wang on

We've recently published our new study about Uncertainty Quantification in Molecular Dynamics (MD) Simulations. Due to the selection of functional forms of interatomic potentials or the numerical approximation, MD simulations may predict different material behavior from experiments or other high-fidelity results. In this study, we used Stochastic Reduced Order Modeling (SROM) to achieve

(1) mechanical behavior of graphene predicted by MD simulations in good agreement with the continuum model which has been calibrated by experiments;

TMS 2020: Fracture Modeling of Composite Materials

Submitted by Saurabh Puri on

Composite materials are increasingly used in industry due to the possibility of tailoring their properties based on the applications. Their greatest advantage is strength and stiffness combined with lightness. However, their optimal design and performance is still limited by the lack of knowledge of physical mechanisms that control their fracture behavior. Machine learning and big data driven approaches have not been extensively studied for fracture behavior predictions.