Journal Club Theme of November 2014: Catalyzed Growth of Semiconductor Nanowires - Multiscale Models
Introduction
Happy Halloween!
In this issue of the Journal Club, I would like to introduce the problem of catalyzed growth of semiconductor nanowires and ways to model it. I would provide web links to only a few articles, hoping that you would download and actually read them so that we can have a more in-depth discussion.