Predictive abilities for stresses in individual inclusions and the matrix by the Mori-Tanaka and PGMT formulation
Both effective properties of composite and the stresses in the individual inclusions and in the matrix are necessary for modelling damage in short fibre composites. Mean field theorems are usually used to calculate the effective properties of composite materials, most common among them is the Mori–Tanaka formulation. Owing to occasional mathematical and physical admissibility problems with the Mori–Tanaka formulation, a pseudo-grain discretized Mori–Tanaka formulation (PGMT) was proposed in literature.