Silica Aerogels: A Review of Molecular Dynamics Modelling and Characterization of the Structural, Thermal, and Mechanical Properties

Submitted by Jingjie Yeo on

https://doi.org/10.1007/978-3-319-50257-1_83-1 The second volume of the Handbook of Materials Modeling is now online: We reviewed the development of new empirical molecular dynamics forcefields, novel methods of generating aerogelsโ€™ percolated backbones, and compelling algorithms for characterizing their structural, mechanical, and thermal properties that have resulted in unprecedented insights into silica aerogels.