Skip to main content

Blog posts

12 Early-Stage Researcher positions on BioImplant - A Marie Curie Training Network Developing Improved Bioabsorable Materials for Medical Implant Applications (3-year PhD)

Submitted by tedvaughan on

 

Project Background: BioImplant Innovative Training Network (ITN) is a European Industrial Doctorate programme that will provide world-class multidisciplinary training to 12 early-stage researchers (ESRs) in the area of bioabsorbable medical implant development.

Webinar- Highlights of Simpleware Software O-2018.12, Jan 16 2019

Submitted by Simpleware on

Join us for this webinar to discover new features and performance improvements in Simpleware software version O-2018.12. Learn about the exciting new features that enhance Simpleware's unparalleled ease-of-use and reliability as a comprehensive solution for all your 3D image processing and analysis workflows

Register today

Ph.D. and postdoctoral openings in the area of non-periodic mechanical metamaterials

Submitted by jenda_z on

One fully-funded Ph.D. student position and two postdoctoral openings are available at the Faculty of Civil Engineering, Czech Technical University in Prague.

Successful candidates will join a newly-formed interdisciplinary group of researchers with expertise in computational mechanics, composite materials, optimization, and mobile and modular robotics. Depending on your research experience and interests, you will contribute either to modeling or experimental investigation of modular pattern-forming mechanical metamaterials built on principles of non-periodic tilings.

10th International Conference on Computational Methods (ICCM2019)

Submitted by Fangsen on

ICCM2019, July 9th-13th, Singapore

 

The conference series originated in Singapore in 2004 by Professor GR Liu, followed by ICCM2007 in Hiroshima, Japan, ICCM2010 in Zhangjiajie, China, ICCM2012 in Gold Coast, Australia, ICCM2014 at Cambridge, England, ICCM2015 at Auckland, New Zealand, ICCM2016 at Berkeley, USA, ICCM2017 at Guilin, China, and ICCM2018 at Rome, Italy.

5th FSSIC Fluid-Structure Sound interactions and Control Symposium, Chania, Greece, 27-30 August 2019

Submitted by GEStavroulakis on

Dear Colleagues,

We have the pleasure to invite you at the 5th Fluid-Structure Sound interactions and Control Symposium in Chania, Crete island, Greece,  from 27-30 August 2019.

The FSSIC Scientific Committee gave us the honour to organise the fifth FSSIC in the beautiful city of Chania. For the organisation, we benefit from the contribution of Professor Georgios Stavroulakis and Dr. Maria Bakatsaki, of the Technical University of Chania.

Journal Club for January 2019: Nanoprecipitation strengthening in high entropy alloys

Submitted by Xiaoyan Li on

Nanoprecipitation strengthening in high entropy alloys

Xiaoyan Li, Jianguo Li

Center for Advanced Mechanics and Materials, Applied Mechanics Laboratory, Department of Engineering Mechanics, Tsinghua University, Beijing 100084, China

Introduction