Postdoc and PhD positions in LEM3, Arts et Métiers ParisTech, Metz-Lorraine
The LEM3 laboratory (UMR 7239) of Arts et Métiers ParisTech, Metz-Lorraine announces 2 postdoc positions and 1 PhD position.
Postdoc position 1
The LEM3 laboratory (UMR 7239) of Arts et Métiers ParisTech, Metz-Lorraine announces 2 postdoc positions and 1 PhD position.
Postdoc position 1
Prof. Liying Jiang at the Mechanical & Materials Engineering Department of University of Western Ontario is seeking a postdoctoral researcher (http://www.eng.uwo.ca/people/lyjiang/)
The Biomedical Engineering (BME) Department at the University of Connecticut invites applications for multiple tenure-track faculty positions at the assistant /associate /full professor level, with an expected start date of August 23, 2014. The attachments include both long and short ads.
Best regards, dmp
Hey,
I am writing a python script for modeling aggregates in a concrete cylinder. I have created a all the particles and and specified section properties to them and to the cylinder.
The procedure I am using is to merge the particles and the cylinder while retaining the boundaries. If the sctions are assigned to the parts before merging, the result is the cylinder with the specified section assignmentsfor each part.
I wrote the code in python but seems like it does not include the section assignment to the new part from merge.
Call for papers – ACT 2014
7th International Conference on Fracture of Polymers, Composites and Adhesives - 14-18 September 2014, Eurotel Victoria, Les Diablerets, Switzerland
We are looking for both experimetal and analytical work, in order to give a balanced view of the subject areas:
- Polymers
- Application of fracture mechanics
- Adhesives
- Composites
For more information or to submit your abstract, go to www.esistc4conference.com
The mechanical behavior of dough, gluten, and
starch was studied in an effort to investigate whether bread dough can be
treated as a two phase (starch and gluten) composite material. Mechanical
loading tests revealed rate-dependent behavior for both the starch and the
gluten constituents of dough. There is evidence from cryo-scanning electron
microscopy that damage in the form of debonding between starch and gluten
occurs when the sample is stretched. In addition, the Lodge material model was
found to deviate from the tension and shear stress-strain test data by a