3-D Microstructure Reconstruction of Polymer Nano-Composite using FIB-SEM and Statistical Correlation Function

Submitted by Azadeh Sheidaei on

 http://www.sciencedirect.com/science/article/pii/S0266353813001012?np=y

Abstract

3-D
reconstruction of Halloysite nanotube (HNT) polypropylene composite has
been performed using two different methods. In the first method,
several slices of the composite material were obtained using focused ion
beam (FIB), and scanning electron microscopy (SEM). A representative
volume element (RVE) of the real material’s micro/nanostructures was

Durability of Reinforced concrete from Composition to Protection

Submitted by shavijabranko on

The 6th International PhD Student Workshop on Durability of Reinforced
Concrete will be held in Delft, The Netherlands, during July 4 and 5,
2013, hosted by TUDelft. After a series of successful workshops, most
recently in Espoo (2012), Madrid (2010) and Guimarães (2009), IPSW2013
will be held under the auspices of RILEM EAC (Educational Activities
Committee), aiming to bring together young researchers in the field of
durability of concrete.

This workshop, aimed at PhD students dealing with concrete durability (in a broad sense), is free of charge.

Mode 1 contours

Submitted by Bharadwaj on

Could anyone tell me why in abaqus,while running a 3D mode 1 fracture analysis,I am not getting the same type of contours on either end of the thickness,i.e.i mean, front and back??While in front side i am getting all the symmetric contour plots,including the red part which shows the highest in the legend,while the back side is devoid of it

Graduate Textbook: Nonlinear Solid Mechanics - Roberval Award

Submitted by Adnan_Ibrahimbegovic on

Mécanique non linéaire des solides déformables:

formulation théorique et résolution numérique par éléments finis

par 

Adnan Ibrahimbegovic

Notes de lecture

par

Philippe Pasquet, Directeur Scientifique SAMTECH

L’un des rares chercheurs et développeurs de la technologie éléments finis appliquée à la résolution de problèmes de mécanique non linéaire des solides

, selon

Minisymposium on "Materials for Extreme Environments: Multi-Scale Experiments and Simulations", SES Annual Meeting (July 28-31

Submitted by Shailendra on

We cordially invite you to participate in the minisymposium "Materials for Extreme Environments: Multi-Scale Experiments and Simulations" at the 50th Society of Engineering Science Annual Technical Meeting (http://www.brown.edu/Conference/ses2013/). The Meeting will be held at Brown niversity, RI, USA during July 28-31, 2013.

FRACTURE-FATIGUE SIMULATION USING MESHFREE METHODS

Submitted by jeetender sing… on

 A power point presentation being prepared for synopsis presentation on

FRACTURE-FATIGUE SIMULATION USING MESHFREE METHODS 

http://www.scribd.com/doc/130329347/Fracture-fatigue-Simulation-Using-M…

Please do give your criticism/ comments/ suggestions to me 

k.jitendrasingh [at] yahoo.com