Skip to main content

Blog posts

Six strategic issues shaping the global future of mechanical engineering

Submitted by Zhigang Suo on

(Initially posted at Applied Mechanics News on 21 May 2006)

The ASME commissioned the Institute for Alternative Futures (IAF), a nonprofit futures think tank, to scan the world for the future of ASME. The IAF report, dated on 30 June 2005, listed the following six strategic issues:

Thickness dependent critical strain in Cu films adherent to polymer substrate

Submitted by Rongmei niu on

For the polymer-supported metal thin films that are finding increasing applications, the critical strain to nucleate microcracks ( εc ) should be more meaningful than the generally measured rupture strain. In this paper, we develop both electrical resistance method and microcrack analyzing method to determine εc of polymer-supported Cu films simply but precisely. Significant thickness dependence has been clearly revealed for εc of the polymer-supported Cu films, i.e., thinner is the film lower is εc . This dependence is suggested to cause by the constraint effect of refining grain size on the dislocation movability.

Innovation and Integration in the Changing Global Higher Education Landscape

Submitted by SHIH Choon Fong on

I’m delighted that mechanicians now have this platform to discuss our work as well as share ideas and perspectives. While we advance knowledge in our field and come up with innovative solutions for engineering and materials problems, I believe that we also have a responsibility to speak on issues of global significance, especially where the power of science and technology can be harnessed to address challenges and issues impacting the world.

Free screen capture softwares for Win and Mac users

Submitted by Jinglei Yang on

I'm writing this post cause it took me much time to find some free softwares that can record activities from screen for Windows and Mac systems. I use both OS at office and lab.

I'm doing some experiments. One is to measure the deformation of microcapsules, both loading curves and deforming capsules via a light microscope displaying on the screen; another is to observe the movement of nano/microcapsules in a cell. For both cases everything is displayed on the screen. I want to record them for kind of live show without using any external recorder and then converting clips.

Combined atomistic and continuum simulation

Submitted by Henry Tan on

H. Tan, 2003
Chapter 12, Combined atomistic and continuum simulation for fracture and corrosion

Comprehensive Structural Integrity (http://www.sciencedirect.com/science/referenceworks/0080437494)
Volume 8: Interfacial and Nanoscale Failure

Constitutive Modelling of Elastomers

Submitted by Mohsin Hamzah on

Rubber or rubber-like materials, or generally elastomers, sustain large elastic deformations. The problems of such cases are non-linear, the non-linearity came from two sources, the first one due to materials, and the second is geomertrical non-linearity. Elastomers are, also, viscoelastic, i.e. time and temperature dependent.

NEW TEXTBOOK ON BIOMECHANICS

Submitted by Alexander A. Spector on

Recently I received a message from the Cambridge University Press regarding a coming text on biomechanics entitled Introductory Biomechanics, From Cells to Organisms. by C. Ross Ethier and Craig A. Simmonds. I ordered an exam copy, went through, and found it very interesting. It covers cellular biomechanics, hemodynamics, circulatory system, ocular biomechanics, muscles and movement, and skeletal biomechanics. Each section has a significant number of problems. I examined closely the part on cellular biomechanics which is one of the main areas of my research and teaching interests, and enjoyed reading it. The cellular mechanics is presented in its interrelation to cell structure and biology (there are nice images of cells and their components to use for teaching). The main techniques of probing the cell, such as micropipette aspiration, AFM, optical tweezers, and magnetic cytometry, are considered. Models of the cytoskeleton (tensergity, foams) are also introduced. The math is limited to linear equations, one-dimensional or axisymmetric problems, but it seems appropriate for the introductory level. In addition, some results of computational (finite element) modeling are also included. I certainly expect that this textbook will be quite useful in my teaching. The web site http://www.cambridge.org/us/catalogue/catalogue.asp?isbn=9780521841122 has more details on the book.

Delamination of stiff islands patterned on stretchable substrates

Submitted by Nanshu Lu on

As another celebration of March Journal Club of Mechanics of Flexible Electronics, this paper has just been submitted.

Abstract 

In one design of flexible electronics, thin-film islands of a stiff material are fabricated on a polymeric substrate, and functional materials are grown on these islands. When the substrate is stretched, the deformation is mainly accommodated by the substrate, and the islands and functional materials experience relatively small strains. Experiments have shown that, however, for a given amount of stretch, the islands exceeding a certain size may delaminate from the substrate. We calculate the energy release rate using a combination of finite element method and complex variable method. Our results show that the energy release rate diminishes as the island size or substrate stiffness decreases. Consequently, the critical island size is large when the substrate is compliant. We also obtain an analytical expression for the energy release rate of debonding islands from a very compliant substrate.