Elastoplastic model for chemo-mechanical behavior of porous electrodes using image-based microstructure
The microstructure of electrodes is intrinsically complex and thus should be determined prior to the analysis of the chemo-mechanical performance during charge/discharge cycles. In this study, a microstructurally resolved, fully coupled chemo-mechanical model was developed to investigate the structure–property relationship of electrodes in the framework of elastoplastic finite deformation.