Hierarchical toughening of bioinspired nacre-like hybrid carbon composite, Jiao, Zhang, Liu, Liu, Zhang, Tang, Liu, Zhang, Carbon, 2021
Novelty/impact/significance:
Hierarchical toughening of bioinspired nacre-like hybrid carbon composite, Jiao, Zhang, Liu, Liu, Zhang, Tang, Liu, Zhang, Carbon, 2021
Novelty/impact/significance:
EML Webinar on November 18, 2020 will be given by Professor Vikram Deshpande, The University of Cambridge. Discussion leader: Professor Lihua Jin, UCLA
Title: Ballistic and blast response of structural materials: lessons from architecting materials
Time: 7 am California, 9:30 am Boston, 2:30 pm London, 10:30 pm Beijing on November 18, 2020
The attached tutorial paper is yet unpublished but I am posting a pre-print since several students I know have found it to be a useful pedagogical resource. You may also access the document on arXiv.
Here is the abstract.
Dear Colleagues,
My group at Peking University proposed a novel mechano-chemical continuum model based on the framework of thermodynamics that can describe the microstructural evolution in metallic glass, and connect it with the macroscopic plastic deformation. The model successfully simulated the shear band instability and dilatancy effects of metallic glass under uniaxial tension and simple shear.
Dear colleagues,
We have published a progress report on hydraulically amplified self-healing electrostatic (HASEL) artificial muscles in Advanced Materials. In this progress report we report the recent developments of HASEL actuators—including materials, designs, fabrication, and control—and discuss many opportunities for future research.
Dear Colleagues,
Event of ASME Technical Committee on Mechanics of Soft Materials 2020:
live symposium and committee meeting
(open access) C. Cissé and M. Asle Zaeem. An asymmetric elasto-plastic phase-field model for shape memory effect, pseudoelasticity and thermomechanical training in polycrystalline shape memory alloys. Acta Materialia 201 (2020) 580-595.
I recommend people with an interest in working with 3D image data and medical devices attend this upcoming webcast between Synopsys Simpleware and CADFEM Medical, which'll take place on Tuesday, November 24th, 2020.
Details here: https://register.gotowebinar.com/register/6605936638572945679?source=IM…
An all-natural bioinspired structural material for plastic replacement, Guan, Yang, Han, Ling, Yu, Nature Communications, 2020
Novelty/impact/significance:
A strong (stiffness 20 GPa and strength 281 MPa), tough (11.5 MPa m1/2), lightweight (1.7 g/cm3), and thermal-resistant (thermal expansion coefficient 7x10-6K-1) composite material is created, using all-natural raw materials through a mass-producible method.