Skip to main content

Fatigue

Postdoc vacancy (2.5 years) on multi-scale modelling of fatigue in 3D printed metals

Submitted by wvpaepeg on

The use of 3D printed metal structures is taking a very fast ramp-up in industry. General Electric has demonstrated the possibility of printing titanium fuel injectors for their LEAP engine, EADS has printed a nacelle hinge bracket for the Airbus A320, Boeing is printing plastic inlet ducts for high-altitude aircrafts, hip implants and other prosthetics are exploiting the design freedom of additive manufacturing (AM),...

Entropy Based Fatigue, Fracture, Failure Prediction and Structural Health Monitoring

Submitted by cemalbasaran on

If you are interested in the most recent advances in physics-based Fatigue, Fracture, Failure Prediction, and Structural Health Monitoring
You may find this publication helpful.

free download site https://www.mdpi.com/books/pdfview/book/3299

Four Fully Funded PhD Positions

Submitted by Mahdi-Bodaghi on

#IPPTPAN in collaboration with Department of Engineering at #NTU is offering four fully supported #PhD positions in the following fields:

 

1) Non-linear thermo-mechanical behaviour of polycrystalline shape memory alloys undergoing complex loadings < https://www.ippt.pan.pl/_download/tem_prac_dok/2020_z_kowalewski_en_1.p… >

 

Postdoctoral Research Fellowship at the University of Udine in Phase-Field modelling of fracture

Submitted by enrico.salvati1 on

I am seeking a full-time Postdoctoral Research Fellow in Phase-Field modelling of fracture to join the Design of Machines group at the Polytechnic Engineering and Architecture Department (DPIA) of the University of Udine. The position is fixed-term for 1 year with funding provided by the European Social Fund (ESF). 

Fatigue of Graphene

Submitted by Teng Cui on

Materials can suffer mechanical fatigue when subjected to cyclic loading at stress levels much lower than the ultimate tensile strength, and understanding this behaviour is critical to evaluating long-term dynamic reliability. The fatigue life and damage mechanisms of two-dimensional (2D) materials, of interest for mechanical and electronic applications, are currently unknown. Here, we present a fatigue study of freestanding 2D materials, specifically graphene and graphene oxide (GO).

Entropy Special Issue

Submitted by cemalbasaran on

 

Deadline for manuscript submissions: 30 November 2019. 

 

Special Issue "Entropy Based Fatigue, Fracture, Failure Prediction and Structural Health Monitoring"

https://www.mdpi.com/journal/entropy/special_issues/fatigue

 

Analytical Models for Fatigue Life Prediction of Metals in the Stress-Life Approach -- phd thesis by Pietro D’Antuono

Submitted by Mike Ciavarella on

dear collegues

  I'd be very grateful if you could have a look, if not a deep reading, at the phd thesis of my last student, playing on classical results on uniaxial fatigue, but with a view of simple, unified perspective on constant and varying amplitude fatigue.  We made large use of e-fatigue.com web site and the data in there.
 
Thanks in advance for any remark.  The final thesis will be submitted in few weeks time.

SEM Fracture and Fatigue Call for Papers

Submitted by Shuman_Xia on

Dear Colleagues,

We invite you to submit a paper to the 2020 Society for Experimental Mechanics (SEM) Annual Meeting in one of the many sessions in the Fatigue and Fracture Track. See below for further information on these sessions, and please forward this to others who may be interested.