Skip to main content

fracture

Symposium on Structure, Plasticity and Fracture of Inorganic Glasses in Paris

Submitted by Erik Bitzek on

Dear Colleagues,



we are organizing a symposium on Plasticity and Fracture in Inorganic Amorphous Materials at 



Condensed Matter in Paris 2014



to be held August 23 to 29, 2014. 



Your experimental or theoretical contributions are highly welcome. 

Please don't hesitate to contact us for more information.



The deadline for abstract submission is  April 1st 2014.



Looking forward to seeing you in Paris in August,



Grants for 3rd International Workshop on Physics Based Material Models and Experimental Observations Cesme/Turkey 2-4 June

Submitted by Kalle Nilsson on

In 2012 and 2013 we organized very successful Workshops on
"Physics-based material models and experimental observations" funded
by the European Union's Enlargement programme. We cordially invite you to
submit an abstract to the 3rd International Workshop on Physics Based
Material Models and Experimental Observations
to be held on 2-4 June
2014 in Cesme-Izmir/Turkey.

MM&FGM14: 13th International Conference on Multiscale Modeling and Functionally Graded Materials

Submitted by Ahmed Elbanna on

Dear Colleagues,

Please consider submitting an abstract to the 13th Internation conference on Multiscale Modeling and Functionally Graded Materials to be held on October 19-22, 2014; in  Taua Resort, SP, Brazi. More information about the conference could be found here:

Normal
0

false
false
false

EN-US
X-NONE
AR-SA

MicrosoftInternetExplorer4

1st invitation to VAL 2015 conference discussing effects of variable amplitude loading

Submitted by pragtic on

Dear iMechanicians,

Let me invite you the 3rd International Conference on Material and Component Performance under Variable Amplitude Loading (VAL 2015) taking place in Prague, Czech Republic in March 23-26, 2015. See the details on its website http://www.val-conf.org.

The conference will discuss among others these primary questions:

Three-dimensional simulation of crack propagation in ferroelectric polycrystals: Effect of combined toughening mechanisms

Submitted by Amir Abdollahi on

We simulate the fracture processes of ferroelectric polycrystals in
three dimensions using a phase-field model. In this model, the grain
boundaries, cracks and ferroelectric domain walls are represented in a
diffuse way by three phase-fields. We thereby avoid the difficulty of
tracking the interfaces in three dimensions. The resulting model can
capture complex interactions between the crack and the polycrystalline
and ferroelectric domain  microstructures. The simulation results show
the effect of the microstructures on the fracture response of the
material. Crack deflection, crack bridging, crack branching and
ferroelastic domain switching are observed to act as the main fracture
toughening mechanisms in ferroelectric polycrystals. Our fully 3-D

17 th National Congress on Theoretical and Applied Mechanics June 15-20 (Michigan State University)

Submitted by Ahmed Elbanna on

Dear all,

I would like to bring to your attention the following minisymposium that is organized as part of the NCTAM 17 (Michigan State University, June 15-20, 2014)

http://www.usnctam2014.org/minisymposium/friction-adhesion-and-fracture…

 

Friction, Adhesion and Fracture: From microscale physics to macroscale response

PhD Position in Fracture Mechanics at the Norwegian University of Science and Technology (NTNU)

Submitted by Zhiliang Zhang on

The Faculty of Engineering Science and Technology (IVT) at the Norwegian University of Science and Technology (NTNU) announces one vacant PhD position in the field of Fracture of Ni-alloys.

ESIS TC4 2014 - Abstract deadline reminder: 25 October 2013

Submitted by Laure Ballu on

7th International Conference on Fracture of Polymers, Composites and Adhesives - 14-18 September 2014, Eurotel Victoria, Les Diablerets, Switzerland

We are looking for both experimetal and analytical work, in order to give a balanced view of the subject areas:

- Polymers

- Application of fracture mechanics

- Adhesives

- Composites

For more information or to submit your abstract, go to www.esistc4conference.com  

 

 

7th International Conference on Fracture Mechanics - Call for Abstracts: deadline 25 October

Submitted by Laure Ballu on

The 7th International Conference in the series will take place once again at Les Diablerets, in Switzerland on 14-18 September 2014.

It organised by the European Structural Integrity Society - Technical Committee 4 on Fracture Mechanics related to Polymers, Polymeric Composites and Adhesives. To submit your abtract, go to http://www.esistc4conference.com/submit-abstract.html