Understanding cementite dissolution in pearlitic steels subjected to rolling-sliding contact loading: A combined experimental and theoretical study

Submitted by chenlei08 on

Cementite dissolution behavior of pearlitic steels subjected to rolling-sliding contact deformation is comprehensively investigated by combining experimental characterization and phase-field modeling.

Tenure-track Assistant Professor Position- Mechanical Engineering-CU Denver

Submitted by Kai Yu on

Assistant Professor-Mechanical Engineering (Position# 11058)

The Department of Mechanical Engineering at the University of Colorado Denver (CU Denver) invites applications for a tenure-track assistant professor position. Applications from candidates in mechanical engineering and related fields will be considered. Individuals with a proven track record in research areas including controls, systems engineering, mechatronics, autonomous systems, solid mechanics and/or experimental fluids-thermal research are encouraged to apply.

Call for Abstracts SEM 2018: Shock & Blast

Submitted by behrad_koohbor on

Dear Colleagues,

 

We would like to invite you to submit an abstract for the ‘Shock & Blast’ session under Track 1: Dynamic Behavior of Materials. This symposium is part of the 2018 SEM Annual Conference & Exposition held at Hyatt Regency Greenville, South Carolina, USA, June 4-7, 2018. This conference marks the 75th Anniversary of SEM and will be a special meeting.

 

Ph.D. and Postdoc Positions in Advanced Materials & Emerging Electronics @ MSU

Submitted by ChangyongCao on

Multiple PhD and Postdocs positions in the fields of advanced materials and energizing electronics are available immediately at Michigan State University. The multi-disciplinary research topics are including mechanics and applications of soft materials and nanomaterials; bioinspired materials, 3D/4D printing; flexible/stretchable/printed electronics; biomaterials and biomechanics; metamaterials and metasurfaces; soft machines and robotics, composite materials etc.

Call for Abstract Submission to 18th USNC/TAM Symposium 104 “Molecular, Cellular, and Tissue Mechanics,”

Submitted by Ying Li on

Dear Colleagues,

You are cordially invited to submit your one-page abstract to our Symposium 104: Molecular, Cellular, and Tissue Mechanics for

18th U.S. National Congress for Theoretical and Applied Mechanics – Jointly Organized with the Chinese Society of Theoretical and Applied Mechanics 

Date & Location:

Hyatt Regency O’Hare (Chicago) from June 5 to June 9, 2018..