Question about curve fitting indentation data with large residual strain
I am trying to use finite element modeling of indentation experiments
to extract hyperelastic material parameters. I am having a dilemma,
when the tissue has residual strain, the model couldn't achieve the
high nonlinear relationship between displacement vs reaction force as
measured in the experiments.
I have tried several strain energy potentials,
1) W=A/B*{exp[B(I1-3)]-1}
2) W=C10(I1-3)+C01(I2-3)
3) W=C10(I1-3)+C20(I1-3)^2+C30(I1-3)^3
4) Arruda-Boyce type model