Simulation of crack behavior of secondary particles in Li-ion battery electrodes during lithiation/de-lithiation cycles

Submitted by zhan-sheng guo on

The loss of connectivity in particle-based LiMO2 (M = Ni, Co, Al, and/or Mn) electrodes due to mechanical failure
and fracture at the interface between primary particles is one of the major causes of capacity fading in Li-ion
batteries (LIBs) after certain electrochemical cycles. In this study, a model of a secondary particle composed
of randomly distributed primary particles is established using a fractal algorithm. The finite element method
with cohesive crack modeling is employed to simulate the intraparticle fracture within the secondary particle.

PhD position at the Institute of Mechanics, OVGU Magdeburg, Germany

Submitted by djuhre on

I have an opening PhD Position at our Institute of Mechanics, Otto von Guericke University Magdeburg (Germany).
The candidate should work in the field of new solution algorithms for complex simulations.
Additionally, the willingnes of teaching (in english as well as in german) is premised.
Attached you will find the corresponding job advertisement.

Modal analysis of historical masonry structures: Linear perturbation and software benchmarking

Submitted by MMSLab-CNR on

https://www.sciencedirect.com/science/article/pii/S0950061818322116 The mechanical behavior of masonry materials has a common feature: a nonlinear behavior with high compressive strength and very low tensile strength. As a consequence, old masonry buildings generally present cracks due to permanent loads and/or accidental events. Therefore, the characterization of the global dynamic behavior of masonry structures should take into account the presence of existing cracks.

Ph.D. Position at Villanova University, US (Computational Fluid Dynamics)

Submitted by Chengyu Li on

A Ph.D. position is available at Villanova University, Department of Mechanical Engineering, to conduct numerical simulations of biological and physiological flows. Financial support for tuition and stipend will be provided. The candidate is expected to start in fall 2019.

The candidate must have previous FORTRAN programming experience and familiar with Linux commands. Previous in-house code development experience is strongly preferred.

 

Qualifications and Skills:

Numerical insights on the structural assessment of historical masonry stellar vaults: the case of Santa Maria del Monte in Cagliari

Submitted by Flavio Stochino on

New Paper: "Numerical insights on the structural assessment of historical masonry stellar vaults: the case of Santa Maria del Monte in Cagliari" Enjoy this free version of the paper!

 

https://rdcu.be/bpvX0

 

Call for Abstract - Frontiers in Built Environment, Earthquake Engineering

Submitted by MMSLab-CNR on

Dear colleagues, Given the recent establishment of the so-called Urban Seismology field and the lack of dedicated journals for the topic, together with Professor Maria Todorovska (University of Southern California, USA), Dr. Riccardo Maria Azzara (INGV, Italy), Dr. Michele Palermo and Dr. Simonetta Baraccani (University of BOlogna, Italy), we would like to establish a network of researchers dealing with this very challenging topic.

Supporting high quality candidates in the coming MSCA-IF call

Submitted by bahmanghiassi on

I am looking to support potential high quality candidates for the coming MSCA-IF call to join my group. The postdoc will work in my group (at University of Nottingham, Faculty of Engineering, Centre for Structural Engineering and Informatics) on an interdisciplinary subject related to materials science or computational mechanics of masonry or concrete structures (new or old materials are possible).

Job vacancy: R&D Engineer (Software Developer), Synopsys, Exeter, UK

Submitted by Simpleware on

Description

This position based in Exeter (UK), would suit a software developer looking to develop novel algorithms for software applications used by international blue chip corporations, research institutions and universities worldwide. For more information about the products you will be working on, please see https://www.synopsys.com/simpleware.html