Skip to main content

Crack initiation patterns at electrode edges in multilayer ferroelectric actuators

Submitted by Amir Abdollahi on

This is the preprint of an article that will appear in Smart Materials and Structures (SMS)

Title: Crack initiation patterns at electrode edges in multilayer ferroelectric actuators

Authors: Amir Abdollahi and Irene Arias, Universitat Politecnica de Catalunya (UPC), Barcelona

 

Abstract:

The ESAFORM 2013 International Conference on Material Forming

Submitted by Robertt Valente on

Dear Colleagues,

Following the last successful events in the past years, the next ESAFORM
Conference on Material Forming (ESAFORM 2013) will represent the 16th
edition of one of the most important and well-established international
research meetings on the material forming field. The conference will be held
at the University of Aveiro, Portugal, from 22 to 24 of April, 2013.

selected papers on fracture in layered materials

Submitted by kilading on

Dear All,

 Currently I am working on the fracture property in layered material and I am focusing on the situation when crack is perpendicular to 

interface. I have read the paper by Dr. Hutchinson and Dr. Suo. If you know any paper that is focusing on the crack perpendicular to the 

interface, please tell me.

 

Thanks and Regards,

 Ding 

Difficulties in indexing monoclinic crystalline materials by wide angle X-ray diffraction

Submitted by Xian Chen on
Choose a channel featured in the header of iMechanica

For monoclinic polycrystalline materials, how can we uniquely index the X-ray diffraction spectrum so that we can calculate the accurate lattice parameters a, b, c and beta? Due to the fact that there are four unknown variables coupled to determine d-spacings, we can not easily read out the lattice parameters until enough diffraction peaks positions are obtained correctly. This leads to two questions

1. How do we get the full diffraction peaks from a monoclinic polycrystalline sample if it is partially textured?

Weyl Geometry and the Nonlinear Mechanics of Distributed Point Defects

Submitted by arash_yavari on

In this paper we obtain the residual stress field of a nonlinear elastic solid with a spherically-symmetric distribution of point defects. To our best knowledge, this is the first nonlinear solution for point defects since the linear solution of Love in the 1920s.

A new postdoctoral position in the mechanics of glassy/amorphous materials

Submitted by Eran Bouchbinder on

A new postdoctoral position in the mechanics of glassy/amorphous materials is
available at the Weizmann Institute of Science. The project will focus on
strongly non-linear phenomena such as cavitation, shear-banding and fracture,
with applications to Bulk Metallic Glasses, and will involve advanced

CM13 - An International Conference on Computational Mechanics - Durham, UK, March 25-27 2013

Submitted by Charles Augarde on

ABSTRACT DEADLINE APPROACHING 31st July 2012

Dear Colleagues

We have received a healthy number of abstracts already for CM13 but we invite you to consider submitting one if you have not done so already. The deadline is 31st July 2012 with full papers due October 15th 2012 (so that they can be reviewed). Please visit the conference website for more details, or contact me directly. I hope some of you can join us in England in 2013.