Skip to main content

Vijay Kumar Sutrakar's blog

Project Associate / PhD Positions: Multiscale Simulation of Nano-Composites for Fatigue & Fracture

Submitted by Vijay Kumar Sutrakar on

Applications are invited for few open positions in the area of
multiscale simulation of fatigue and fracture of advanced alloys and
nano-material based composites. Primary focus of this research is investigation
of fatigue and fracture behavior of nanomaterials and to develope various
constitutive models for continuum, based on large scale atomistic simulations.
Research effort will include development of analysis and design methods toward
improving material/structural behaviour using computer simulation. Interested
candidates should have preferably MTech/ME degree in
mechanical/civil/aerospace/material engineering discipline with good knowledge

Temperature–pressure-induced solid–solid 〈100〉 to 〈110〉 reorientation in FCC metallic nanowire

Submitted by Vijay Kumar Sutrakar on

 I would like to share our recent research work on FCC metallic nanowires, which is published in Journal of Physics : Condensed Matters (IOP) . The abstract of the paper is given below. Further details can be found at

Vijay Kumar Sutrakar et al 2012 J. Phys.: Condens. Matter 24 015401 

doi:10.1088/0953-8984/24/1/015401


Abstract: 

Designing copper–zirconium based nanowires for improving yield strength and plasticity via configuring surface atoms

Submitted by Vijay Kumar Sutrakar on

Following our previous work on Cu-Zr nanowire system, in this paper we have shown improvement in various thermo-mechanical properties of nanowire via manipulating the surface atoms. The paper titled "Designing copper–zirconium based nanowires for improving yield strength and plasticity via configuring surface atoms" by Vijay Kumar Sutrakarand D Roy Mahapatra has been published in Journal of Nanoparticle Research. The paper can be downloaded from
http://www.springerlink.com/content/j2786222101mn711/

Universal Stability and Temperature Dependent Phase Transformation in Group VIIIB–IB Transition Metal FCC Nanowires.

Submitted by Vijay Kumar Sutrakar on

I want to share our recent research work on FCC metallic nanowires, which is published in Journal of Physical Chemistry - C (ACS Publications). The abstract of the paper is given below. Further details can be found at " Sutrakar et al  J. Phys. Chem. C, 2011, 115 (21), pp 10394–10398

DOI: 10.1021/jp2006815

 

Stress-induced phase transformation and pseudo-elastic/pseudo-plastic recovery in intermetallic Ni–Al nanowires

Submitted by Vijay Kumar Sutrakar on

Dear friends,

I want to share our recent research work on NiAl nanowire, which is published in Nanotechnology, IOP publishing. The abstract of the paper is given below. Further details can be found at "Vijay Kumar Sutrakar et al 2009 Nanotechnology 20 295705 (9pp)   doi: 10.1088/0957-4484/20/29/295705"

 

Stress-induced martenstic phase transformation in Cu-Zr nanowires

Submitted by Vijay Kumar Sutrakar on

Hi Friends

I want to share some of our recent research work on the stress induced phase transformation of CuZr nanowire which is published in Materials Letters.

http://dx.doi.org/10.1016/j.matlet.2009.02.064