A new model to predict grain nucleation during dynamic recrystallization

Submitted by ystarase on

http://www.magnet.ubc.ca/wiki/images/5/5a/Abhijit_Mg2012.pdf

 

Deformation in metals and alloys is accompanied by high hardening rates and high dislocation 

content. Static annealing of deformed metals or forming operations at elevated temperatures can 

lead to static and dynamic recrystallization (SRX and DRX). The resultant texture and hence the 

properties of such a material are determined by the nucleation and growth of recrystallized grains 

ABAQUS model of polycrystal plasticity

Submitted by lu_1989 on

Hi everyone 

I am learning the polycrystalline crystal plasticity and testing material in ABAQUS and UMAT. Now I am trying to build a RVE by using the truncated octahedrons as the grain shape or Voronoi tessellations.

For truncated octahedrons, I built a truncated octahedrons and assembled them into the grain aggregate in the .inp file, and assign orientations in the UMAT based on the part's name. However, I found it hard to define their interaction between grains. What is their interaction properties and how to define the contact pair in an automatic way?

Hardness Evaluation of Biological Tissue Using Nanoindentation

Submitted by NANOVEA on

The ability to accurately measure mechanical properties, using Nanoindentation, in the fields of Life Science has recently become an important aspect of many current studies. In some cases, understanding the mechanical properties of soft biological surfaces have helped uncover the mechanical effects of diseases. Understanding mechanical properties provides a context for identifying the local mechanical behavior linked to specific changes. It is also critical in the development of artificial bio-materials.

New Ebook on Elastic Solids at Amazon

Submitted by Carl T. Herakovich on

This treatise provides a broad overview of the definitions of
fundamental quantities and methods of analysis for the use of solid materials
in structural components. The presentation is limited to the linear elastic
range of material behavior where there is a one to one relationship between
load and displacement.  Fundamental
methods of analysis and typical results for structures made of elastic solid materials
subjected to axial, bending, torsion, thermal, and internal pressure loading;

Eulerian Analysis in impact phenomena

Submitted by mikelebof on

Hi friends,

 Does anybody know what this error mean?

The general contact definition is empty. The definition must include at least one surface. If *CONTACT EXCLUSIONS was defined, check whether the *CONTACT EXCLUSIONS option was specified correctly. Additionally, check whether PURE MASTER-SLAVE formulation is applied to any self-contact situations.

Faculty Position (in Mechanics) at Graz University of Technology, Austria

Submitted by Manfred H Ulz on

There is an open faculty position at the Department of Mechanical Engineering, Graz University of Technology, Austria in the field of strength of materials.

More information about the position and the application instruction may be found here:

 http://mibla.tugraz.at/12_13/Stk_18/18.html#255

As the position will involve undergraduate teaching in German, candidates need to be fluent in German (hence, the description is in German only).