Skip to main content

Plasticity

ES 246 Project: Large Deformation Plasticity of Amorphous Solids, with Application and Implementation into Abaqus

Submitted by Kristin M. Myers on

node/add/imageI propose to investigate an elastic-viscoplastic constitutive model proposed by Anand and Gurtin [1] for the large deformation of amorphous solids.  Specifically, I will present the constitutive framework proposed for elastic-plastic amorphous materials, I will implement the constitutive equations into Abaqus/Explicit, and I will compare numerical results with experimental results for polycarbonate [2]. 

 

Void-induced strain localization at interfaces

Submitted by Anonymous (not verified) on

We published this paper in APL on a study of the deformation near interfaces. It provides insight in the strain localization at the interface and its influence on the deformation in bulk metals. 

Abstract An optical full-field strain mapping technique has been used to provide direct evidence for the existence of a highly localized strain at the interface of stacked Nb/Nb bilayers during the compression tests loaded normal to the interface. No such strain localization is found in the bulk Nb away from the interface. The strain localization at the interfaces is due to a high void fraction resulting from the rough surfaces of Nb in contact, which prevents the extension of deformation bands in bulk Nb crossing the interface, while no distinguished feature from the stress-strain curve is detected.

Plastic deformation of freestanding thin films: Experiments and modeling

Submitted by Anonymous (not verified) on

This is a paper we recently published in JMPS on a study of the mechanical properties on thin films comparing experimental results with discrete dislocation simulations. It provides insight in the strengthening that occurs in thin metal films when surface or interface effects become important.

The abstract is below; the full paper can be downloaded from here

Abstract - Experimental measurements and computational results for the evolution of plastic deformation in freestanding thin films are compared. In the experiments, the stress–strain response of two sets of Cu films is determined in the plane-strain bulge test. One set of samples consists of electroplated Cu films, while the other set is sputter-deposited. Unpassivated films, films passivated on one side and films passivated on both sides are considered. The calculations are carried out within a two-dimensional plane strain framework with the dislocations modeled as line singularities in an isotropic elastic solid. The film is modeled by a unit cell consisting of eight grains, each of which has three slip systems. The film is initially free of dislocations which then nucleate from a specified distribution of Frank–Read sources. The grain boundaries and any film-passivation layer interfaces are taken to be impenetrable to dislocations. Both the experiments and the computations show: (i) a flow strength for the passivated films that is greater than for the unpassivated films and (ii) hysteresis and a Bauschinger effect that increases with increasing pre-strain for passivated films, while for unpassivated films hysteresis and a Bauschinger effect are small or absent. Furthermore, the experimental measurements and computational results for the 0.2% offset yield strength stress, and the evolution of hysteresis and of the Bauschinger effect are in good quantitative agreement.

ES 246 projects

Submitted by Anonymous (not verified) on

Each student creates a project that addresses a phenomenon or issue in plasticity theory, and presents it in class after the winter break. The scope of the projects is very wide: experimental, computational, or a critical discussion of one or more papers. The project contributes 30% of the grade, distributed as follows:

  • 5%: November 30 Thursday. Post your project proposal in iMechanica.
  1. Title. ES 246 project: e.g. Plastic buckling of plates.
  2. Tags. Use the following tags: ES 246, plasticity, Fall 2006, project
  3. Body. (i) Describe the project. (ii) Cite at least 1 journal article.
  • 5%: December 7 Thursday. Post a comment to critique the project proposal of at least 1 classmate.

The 13th International Conference on Experimental Mechanics

Submitted by Horacio Espinosa on

Dear Colleagues:


The 13th International Conference on Experimental Mechanics (ICEM13, http://www.icem13.gr) will be held on July 1-6, 2007 in Alexandroupolis, Greece. It is our pleasure to announce that the Conference will include a special symposium organized by us entitled, “Plasticity, Fracture and Fatigue at the Micro and Nano Scales,” which will focus on recent developments in this area within the larger scope of assessing research needs in a variety of applications of interest.