Abaqus - cohesive concrete and epoxy
Hi,
I was browsing through this forum which I find very helpful.
I am trying to model a simple shear pull out test by simulating debonding in abaqus.
epoxy is bonded between concrete and frp.
i am pulling frp from one end by applying a load while other end of concrete is fixed.
epoxy is modeled as cohesive with quad damage and traction
interaction has been defined as hard contact, cohesive and damage (initiation, evolution and stabilization).
automatic stabilization is also provided by inputing the damping factor.
Open Ph.D. positions at UT-Arlington
There are three Ph.D. positions opening in our group: one in Cell/Tissue Mechanics, one in Mechanics of Energy Storage Materials, and the last in Metamaterials. We would like to fill these positions as soon as in the Spring, 2012. Qualified candidates with a M.S. degree in Mechanical Engineering or related discipline are welcome to apply. If interested, please send a copy of C.V. to boyang [at] uta.edu. Also, please indicate which position you apply.
Special Academic Offer -- ADINA
Dear Colleague,
1. As you may know, ADINA is extensively used in teaching and research
at universities all around the world. If you are not already a university user,
you may be interested in the following announcement:
http://www.adina.com/educ.shtml
2. For an overview of the comprehensive multiphysics capabilities of ADINA see
the following page:
XFEM into Diffpack for fracture mechanics
A 6 month post is available, either as recruited staff or consultant for 3D fracture mechanics applications within Diffpack (inuTech) http://www.inutech.de/
at Cardiff University.
The profile of the candidate:
Mandatory criteria
-strong C++coding experience
-knowledge of numerical methods
Desirable criteria
-Diffpack experience
-XFEM experience
Depending on performance, the post can be extended through other contracts (see posts below).
Does pure shear stress exist?
Call for abstracts: Computational mechanics of cells, tissues, and biomaterials (ECOMASS 2012)
Call for Abstracts (Deadline: December 15, 2011)
As a part of ECCOMAS 2012 (European Congress on Computational Methods in Applied Sciences and Engineering)
Submit your Abstract (Choose mini-symposium MS114)
Postdoc positions in Center for Nano and Micro Mechanics (CNMM) at Tsinghua University, Beijing, China
There are TEN openings for postdoctoral positions in the Center for Nano and Micro Mechanics (CNMM) at Tsinghua University. The Center is an interdisciplinary innovation center supported by Tsinghua University, with specially focused interests in nanomaterials, nanodevices, nano-enabled energy and environmental applications. More details about the faculties and research area can be found at http://cnmm.tsinghua.edu.cn.
a question about Euler beam in ABAQUS
To eliminate the unwanted axial strain constraint, in Abaqus the stretch dL/dS at the node of each such element is taken as an internal variable, local to the element (a third internal node is created for this purpose, and so it is not shared with neighboring elements.)
Above paragraph is excerpted from chapter about Euler beam theory in ABAQUS theory manual.