We are seeking a highly motivated individual to join our Vancouver research institute. This is a two-year industrial postdoctoral fellow position, which could lead to permanent employment.The successful incumbent will work with a multi-disciplinary team of scientists to develop computer models to predict mechanical properties of wood and paper products.

Abaqus / polymer simulation

Submitted by poucinette on
Hi all,



I'm trying to model a peel T test on a composite material composed of steel and polymer (polypropylen) on Abaqus 6.7. Between these parts, there are cohesive elements COH3D8.

I have a problem with my model and I don't understand it. You can visualize my results in attachs files.

For understand this draw, a few precisions:

The elements in white has just here to guide the materials.

In B (cf attachs files), the nodes are embedded.

In A I applied a velocity.

modeling in abaqus using dynamic/explicit

Submitted by Anonymous (not verified) on

HI ,

I am Ashutosh..

i m a student of Mtech in cad/m from MNNIT, ALLAHABAD, INDIA.

I am working on my thesis for mtech which is to model erosive wear of materials under particle impact.

pls i need help on it as how can i model and simulate in abaqus/explicit.

 

hoping a reply..

regards

ashutosh 

XFEM Ph.D. Position Computational Mechanics Reservoir Modelling Collaboration with Industry, Schlumberger

Submitted by Stephane Bordas on

PhD available at the University of Glasgow entitled ‘Numerical Simulation of Fault Evolution in Oil Reservoirs’ 

EPSRC Case Award with Schlumberger - £15,500 per annum + fees. 


Postdoc position available at MIT / bioinspired thermal management

Submitted by Markus J. Buehler on

A postdoctoral associate position at MIT is available immediately, focused on the analysis and development of bioinspired, adaptive thermal management structures, by using theoretical and atomistic multi-scale modeling and simulation.

Seeking POSTDOC position on Impact analysis, Composite manufacturing, FEM, LS-DYNA, ANSYS, ABAQUS

Submitted by Lakshya J Deka on

I am lakshya,  a Phd student in materials engineering dept at University of Alabama in Birmingham. I will be graduating this summer, 2008. I have been working in composite field (manufacturing, testing, FEM, LS-DYNA) for almost 4 years. My resume has been attached herewith . Please contact me at lakshya [at] uab.edu (lakshya[at]uab[dot]edu) or 2053709560.

Illustration of Consistent Tangent Tensor

Submitted by Attila Kossa on

I am looking for a good geometric illustration of the consistent tangent tensor (corresponding to a stress update procedure).

The theory is "clear" for me, but sometimes i am confused when i wanted to imagine the illustration of the difference between the consistent tangent and the continuum tangent tensors.

Could someone recommend me a textbook or paper that presents a good schematic illustration ?

Best Regards!

 

problem in full transient analysis

Submitted by iraj4u on

hi friends

i have problem in full transient analysis in ANSYS 11.0

kindly give me solution.

i have data .....

BEAM FOR IMPACT LOAD 

lenth=144 inch 

area=120 sq inch 

moment of inrtia=1000 inch rest to four

depth=10 inch

elastic modulas=3605 kips per sq inch

density of material=8.6805E-5  kips per cubic inch

FOR SOLUTION..(force 23.8 kips is linearly decreases from time = 0 to 0.042 at centre of the beam)

at time = 0 sec , force = -23.8 kips