Skip to main content

Blog posts

Webinar, USACM, TTA-Uncertainty Quantification and Probabilistic Modeling:: Title: Measuring dataset similarity in clustering-based, uncertainty-aware federated learning. Speaker: Prof. Chao Hu, University of Connecticut

Submitted by susanta on

This is a reminder that our next monthly webinar is December 5, 3-4pm EST. The speaker will be Associate Professor Chao Hu from University of Connecticut. We are hoping the format will promote a lively interactive discussion and engage both junior and senior members of our community. Look forward to seeing you there.

Monthly Webinar by USACM, TTA-Uncertainty Quantification and Probabilistic Modeling

December 5; 3pm EST

Speaker: Associate Professor Chao Hu, University of Connecticut

Postdoctoral fellowship in Computational Fracture Mechanics at Duke

Submitted by John E. Dolbow on

I am happy to announce that a postdoctoral fellowship is available in the Dolbow Research Group at Duke University, working in the area of computational fracture mechanics.  The fellowship provides the opportunity to work on an emerging class of complete fracture models that incorporate the three ingredients that are necessary to be predictive with elastic brittle materials: their elasticity, their fracture toughness, and their strength.  

Department Chair Search : New Jersey Institute of Technology (R1) Mechanical and Industrial Engineering

Submitted by Dibakar Datta on

The Department of Mechanical and Industrial Engineering at the New Jersey Institute of Technology (R1) is seeking a visionary leader to serve as Department Chair. If you are interested in this exciting leadership opportunity, please apply here :
https://njit.csod.com/ux/ats/careersite/1/home/requisition/7605?c=njit

We kindly request you to share this opportunity with anyone who might be a strong candidate for this role.

Thank you,
Search Committee

Bažant-Le-Kirane Paradox of fatigue failure in engineering materials

Submitted by g2mahendra on

Author: Mahendra Gattu, Department of Civil Engineering, NIT-Rourkela-769008.

Abstract

The problem of fracture in quasi-brittle materials is strongly linked with a zone of micro-cracking known as the fracture process zone (FPZ). For monotonic loading, the material length scale parameter D0 is used in strength scaling law to describe the transition from strength criteria to linear elastic fracture mechanics criteria.

Associate Professor position in Solid Mechanics at the University of Oxford

Submitted by Laurence Brassart on

The Department of Engineering Science at the University of Oxford intends to appoint an Associate Professor of Engineering Science (Solid Mechanics) with effect from 1 October 2025 (or as soon as possible thereafter). The successful candidate will work at the Department of Engineering Science (Central Oxford) and will be offered a Tutorial Fellowship at Pembroke College. The appointment will be initially for five years at which point, upon completion of a successful review, the post-holder will be eligible for reappointment to the retiring age.

PhD opening at UCLA

Submitted by Lihua Jin on

The Mechanics of Soft Materials Lab (https://www.msm.seas.ucla.edu/) led by Prof Lihua Jin in the Mechanical and Aerospace Engineering at University of California, Los Angeles (UCLA) has a PhD opening to be filled in 2025 fall. Successful candidates are expected to work on modeling, simulations, and experiments of soft materials, soft tissue and soft robots. The ideal candidates will be highly motivated with a strong background in solid mechanics and computation, and be fluent in spoken and written English.